Table 2 Structural parameters of ZnO-CNT annealed at 300 °C

From: Analysis on the effect of ZnO on Carbon nanotube by spray pyrolysis method

Position FWHM D A° Plane spacing Diffraction lines Grain Size (nm) Dislocation density (δ) (1015) lines/m2 Strain (ε) (10−3)
Std. Obs.
27.5053 0.1673 3.348 3.2429 3.348 005 51.085 0.3832 0.7633
42.7882 0.4015 2.11 2.1134 2.1100 - 22.206 2.0279 1.1407
45.1937 0.5333 2.061 2.0064 2.0615 - 16.798 3.5438 1.4346
51.2405 0.6691 1.896 1.7829 1.8961 008 13.759 5.2818 1.5565