Table 1 Physical and mechanical properties of Al2O3–SiCw–TiC (Patel et al. 2009a, 2009b, 2009c)

From: Processing of Al2O3–SiCw–TiC ceramic composite by powder mixed electric discharge grinding

Hardness (Hv) Fracture toughness KIC (MPa (m) 0.5) Thermal conductivity k (W/mK at 400°K) Electrical Resistivity (Ωcm) Density ρ (g/cm3)
2400 9.6 ± 0.6 63 0.009 3.915