Fig. 10From: Rheonomic phenomenon shrinkage of holes drilled in fibreglass and carbon fibre-reinforced polymer compositesDependence of hole diameter immediately after drilling (blue and grey bars) and in 48 h after drilling (orange and yellow bars) with the use of diamond drill and HAM carbide drill for KMU-4E material under different machining modesBack to article page