Skip to main content

Table 5 DMA properties of EPDM, NBR and their composites

From: Effect of graphene on polar and nonpolar rubber matrices

Compounds (phr) Storage Modulus (MPa) Reinforcement Coefficient (C)
Glassy region (-15 °C) Rubbery region (40 °C)
NBR 55.7 3.2 1
NBR-GO-1 44.5 3.9 0.66
NBR-rGO-1 46.0 3.6 0.73
EPDM 3.7 3.2 1
EPDM-GO-1 4.1 3.7 0.95
EPDM-rGO-1 4.4 4.0 0.95